strength of material lab

strength of material lab

Creep Testing Machine

Creep Testing Machine

Table unit for the investigation of the creep  behavior of different materials Flat specimens made of lead and PP Specimen cross-section 2 - 5 mm, measured length 25 mm
Tensile stress range 5...25N/mm2
Position measurement gauge 0...10mm
resolution 0.01mm
Experiments above or below room temperature possible with conditioning box
Specimen
material: lead, PP
cross-section: 2 - 5 mm
measured length: 25mm
Tensile stress range: 5.25N/mm2
Position measurement
-range: 0...10mm
-resolution 0.01 mm